Nerezová ocel 316/316L – vysoce-výkonná korozní-slitina
Mar 09, 2026
Zanechat vzkaz



Dostupné tloušťky pro Alloy 316/316L:
| 3/16" | 1/4" | 5/16" | 3/8" | 7/16" | 1/2" | 9/16" | 5/8" | 3/4" | 7/8" | 1" | 1 1/8" |
| 4,8 mm | 6,3 mm | 7,9 mm | 9,5 mm | 11,1 mm | 12,7 mm | 14,3 mm | 15,9 mm | 19 mm | 22,2 mm | 25,4 mm | 28,6 mm |
| 1 1/4" | 1 3/8" | 1 1/2" | 1 5/8" | 1 3/4" | 2" | 2 1/4" | 2 1/2" | 2 3/4" | 3" | 3 1/4" | 3 1/2" |
| 31,8 mm | 34,9 mm | 38,1 mm | 41,3 mm | 44,5 mm | 50,8 mm | 57,2 mm | 63,5 mm | 69,9 mm | 76,2 mm | 82,6 mm | 88,9 mm |
| 3 3/4" | 4" | 4 1/4" | 4 1/2" | 4 3/4" | 5" | 5 1/4" | 5 1/2" | 5 3/4" | 6" | ||
| 95,3 mm | 101,6 mm | 108 mm | 114,3 mm | 120,7 mm | 127 mm | 133,4 mm | 139,7 mm | 146,1 mm | 152,4 mm |
Chemická analýza
Hmotnost % (všechny hodnoty jsou maximální, pokud není uvedeno jinak)
| Živel | 316 | 316L |
|---|---|---|
| Chrom | 16,0 min.-18,0 max. | 16,0 min.-18,0 max. |
| Nikl | 10,0 min.-14,0 max. | 10,0 min.-14,0 max. |
| Molybden | 2,00 min.-3,00 max. | 2,00 min.-3,00 max. |
| Uhlík | 0.08 | 0.030 |
| Mangan | 2.00 | 2.00 |
| Fosfor | 0.045 | 0.045 |
| Sulfer | 0.03 | 0.03 |
| Křemík | 0.75 | 0.75 |
| Dusík | 0.1 | 0.1 |
| Železo | Váhy | Váhy |